콘텐츠 본문
논문 해외 국제전문학술지(SCI급) The effects of humidity on the self-discharge properties of Li(Ni1/3Co1/3Mn1/3)O2/graphite and LiCoO2/graphite lithium-ion batteries during storage
- 학술지 구분 국제전문학술지(SCI급)
- 게재년월 2017-01
- 저자명 Seoungwoo Byun, Joonam Park, Williams Agyei Appiah, Myung-Hyun Ryou, Yong Min Lee
- 학술지명 RSC Advances
- 발행처명 Royal Society of Chemistry
- 발행국가 해외
- 논문언어 외국어
- 전체저자수 5
- 논문 다운로드 링크(외부) DOI: 10.1039/C6RA28516C
- 연구분야 공학 > 화학공학
논문 초록 (Abstract)
To investigate the effects of the exposure of battery tabs to humidity on the self-discharge properties of full-cell type lithium-ion batteries (LIBs), we assembled two different types of LIBs, composed of NCM/graphite or LCO/graphite, and compared their discharge retention abilities after storage in humid conditions (90% relative humidity (RH)) with and without battery tab protection. Regardless of the type of cathode active materials, tab protection improved the calendar lives of LIBs. For NCM/graphite, battery tab protection shows an approximate 50% improvement in the discharge capacity compared to the case without battery tab protection after storage in humid conditions (51.1% and 34.6% of the initial discharge capacity for tab-protected and non-protected LIBs, respectively). In contrast, LCO/graphite reveals a smaller change in the discharge capacity retention for the same experimental condition because they show superior capacity retention abilities regardless of battery tab protection (85.6% and 82.0% retention of the initial discharge capacity for tab-protected and non-protected LIBs, respectively). We suggested that these results come from the induction effect of polar water molecules, which pulls electrons to the battery tab side, resulting in lithium ion loss from the graphene layers to the liquid electrolyte.